MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
SABIC LEXAN™ FR 505R PC (Americas)
Categories: Polymer; Thermoplastic; Polycarbonate (PC)

Material Notes: LEXAN 505R Polycarbonate (PC) is an injection moldable non-chlorinated and non-brominated flame retardant grade that is10% glass fiber filled. It has a UL94 V0@1.5mm rating and is available in various opaque color options. This is an alternative to LEXAN 500, 500R, 500RS, 500ECR.

Information provided by SABIC

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.26 g/ccASTM D792
Density 1.25 g/ccISO 1183
Water Absorption 0.12 %24 hours; ASTM D570
 0.31 %23°C/sat; ISO 62
Moisture Absorption 0.130 %23°C / 50% RH; ISO 62
 0.130 %50% RH, 24 hrs; ASTM D570
Moisture Absorption at Equilibrium 0.31 %ASTM D570
Linear Mold Shrinkage, Flow 0.0020 - 0.0060 cm/cmSABIC method
 0.0050 - 0.0070 cm/cm
@Thickness 3.20 mm
SABIC method
Melt Flow 7.0 g/10 min
@Load 1.20 kg,
Temperature 300 °C
ASTM D1238
 7.0 g/10 min
@Load 1.20 kg,
Temperature 300 °C
cm³/10 min; ISO 1133
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell M 85ASTM D785
Hardness, Rockwell R 124ASTM D785
Ball Indentation Hardness 115 MPaISO 2039-1
Tensile Strength at Break 45.0 MPa5 mm/min; ISO 527
 48.0 MPa5 mm/min; ASTM D638
Tensile Strength, Yield 60.0 MPa5 mm/min; ISO 527
 63.0 MPa5 mm/min; ASTM D638
Elongation at Break 7.0 %5 mm/min; ISO 527
 12 %5 mm/min; ASTM D638
Elongation at Yield 3.0 %5 mm/min; ASTM D638
 5.0 %5 mm/min; ISO 527
Tensile Modulus 3300 MPa1mm/min; ISO 527
 3930 MPa5 mm/min; ASTM D638
Flexural Strength 108 MPabrk, 1.3 mm/min, 50 mm span; ASTM D790
Flexural Yield Strength 95.0 MPa2 mm/min; ISO 178
Flexural Modulus 3400 MPa2 mm/min; ISO 178
 3530 MPa1.3 mm/min, 50 mm span; ASTM D790
Izod Impact, Notched 107 J/mASTM D256
 80.0 J/m
@Temperature -30.0 °C
ASTM D256
Izod Impact, Unnotched 1602 J/mASTM D4812
Izod Impact, Notched (ISO) 8.00 kJ/m²80*10*4; ISO 180/1A
 10.0 kJ/m²80*10*3; ISO 180/1A
 8.00 kJ/m²
@Temperature -30.0 °C
80*10*4; ISO 180/1A
 8.00 kJ/m²
@Temperature -30.0 °C
80*10*3; ISO 180/1A
Izod Impact, Unnotched (ISO) NB80*10*3; ISO 180/1U
 NB80*10*4; ISO 180/1U
 130 kJ/m²
@Temperature -30.0 °C
80*10*3; ISO 180/1U
 NB
@Temperature -30.0 °C
80*10*4; ISO 180/1U
Charpy Impact Unnotched NBEdgew 80*10*4 sp=62mm; ISO 179/1eU
 NBEdgew 80*10*3 sp=62mm; ISO 179/1eU
 NB
@Temperature -30.0 °C
Edgew 80*10*4 sp=62mm; ISO 179/1eU
 NB
@Temperature -30.0 °C
Edgew 80*10*3 sp=62mm; ISO 179/1eU
Charpy Impact, Notched 9.00 kJ/m²Edgew 80*10*4 sp=62mm; ISO 179/1eA
 10.0 kJ/m²Edgew 80*10*3 sp=62mm; ISO 179/1eA
 15.0 kJ/m²ISO 179/2C
 9.00 kJ/m²
@Temperature -30.0 °C
Edgew 80*10*3 sp=62mm; ISO 179/1eA
Dart Drop, Total Energy 61.0 JASTM D3763
Taber Abrasion, mg/1000 Cycles 11CS-17, 1 kg; SABIC method
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity >= 1.00e+15 ohm-cmIEC 60093
Surface Resistance >= 1.00e+15 ohmROA; IEC 60093
Dielectric Constant 2.8
@Frequency 1e+6 Hz
IEC 60250
 2.9
@Frequency 50.0 - 60.0 Hz
IEC 60250
Dielectric Strength 16.0 kV/mm
@Thickness 3.20 mm
in oil; IEC 60243-1
 25.0 kV/mm
@Thickness 1.60 mm
in oil; IEC 60243-1
 33.0 kV/mm
@Thickness 0.800 mm
in oil; IEC 60243-1
Dissipation Factor 0.0010
@Frequency 50.0 - 60.0 Hz
IEC 60250
 0.010
@Frequency 1e+6 Hz
IEC 60250
Comparative Tracking Index 175 VIEC 60112
 175 - 250 VUL 746A
Hot Wire Ignition, HWI 30 - 60 secUL 746A
High Amp Arc Ignition, HAI 15 - 30 arcsUL 746A
High Voltage Arc-Tracking Rate, HVTR 80.0 - 150 mm/minUL 746A
 
Thermal PropertiesOriginal ValueComments
CTE, linear, Parallel to Flow 40.0 µm/m-°C
@Temperature 23.0 - 80.0 °C
ISO 11359-2
 46.8 µm/m-°C
@Temperature -40.0 - 40.0 °C
ASTM E831
CTE, linear, Transverse to Flow 70.0 µm/m-°C
@Temperature 23.0 - 80.0 °C
ISO 11359-2
 84.6 µm/m-°C
@Temperature -40.0 - 40.0 °C
ASTM E831
Specific Heat Capacity 1.21 J/g-°CASTM C 351
Thermal Conductivity 0.200 W/m-KASTM C177
 0.210 W/m-KISO 8302
Hot Ball Pressure Test 125 °CIEC 60695-10-2
Deflection Temperature at 0.46 MPa (66 psi) 142 °CFlatw 80*10*4 sp=64mm; ISO 75/Bf
 144 °CEdgew 120*10*4 sp=100mm; ISO 75/Be
 143 °C
@Thickness 3.20 mm
unannealed; ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 135 °CFlatw 80*10*4 sp=64mm; ISO 75/Af
 136 °C1.8 MPa Edgew 120*10*4 sp=100mm; ISO 75/Ae
 138 °C
@Thickness 3.20 mm
unannealed; ASTM D648
 136 °C
@Treatment Temp. 120 °C,
Time 7200 sec
annealed; ISO 75/Ae
Vicat Softening Point 141 °CRate B/50; ISO 306
 143 °CRate B/120; ISO 306
 149 °CRate B/50; ASTM D1525
UL RTI, Electrical 130 °CUL 746B
UL RTI, Mechanical with Impact 130 °CUL 746B
UL RTI, Mechanical without Impact 130 °CUL 746B
Flammability, UL94 V-0
@Thickness 1.50 mm
UL 94
 5VB
@Thickness 2.00 mm
UL 94 by SABIC-IP
 5VA
@Thickness 3.00 mm
UL 94
Oxygen Index 37 %ISO 4589
Glow Wire Test 825 °C
@Thickness 1.00 mm
IEC 60695-2-13
 960 °C
@Thickness 1.00 mm
IEC 60695-2-12
 
Processing PropertiesOriginal ValueComments
Processing Temperature 60.0 - 80.0 °CHopper Temperature
Nozzle Temperature 280 - 310 °CInjection Molding
Zone 1 270 - 300 °C
Zone 2 280 - 310 °C
Zone 3 290 - 320 °C
Melt Temperature 290 - 320 °C
Mold Temperature 80.0 - 120 °C
Drying Temperature 120 °CInjection Molding
Dry Time 2.00 - 4.00 hourInjection Molding
Moisture Content 0.020 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PSABI10587 / 244054

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.