MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Evonik Modifier 705 Plasticizer
Categories: Other Engineering Material

Material Notes: Modifier 705 and Modifier 715 are SiH-terminated polydimethyl siloxanes which are used as plasticizers in addition-curing silicones. Due to their difunctional structure, these products do not react by cross-linking, but by extending the chains of vinyl-terminated silicone polymers (Polymer VS). Use of the modifiers reduces the crosslinking density and therefore the elastomer hardness.

Application: Use of the modifiers allows obtaining products with a low Shore hardness, even when using low-viscosity vinyl polymers. These modifiers are therefore used in formulations that have a low viscosity prior to crosslinking and should have low Shore hardness after crosslinking. Another important modifier application is the formulation of silicone gels. When working with two-component silicone formulations, it must be ensured that Pt-catalyst (e. g. Catalyst 500 series) and modifier are kept strictly apart.

Information provided by Evonik

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.00 g/cc
Viscosity 500 cP
 
Optical PropertiesOriginal ValueComments
Refractive Index 1.405
 
Descriptive Properties
AppearanceClear, colorless liquid
Content0.16 mmol/gSiH

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Evonik VESTINOL® INB Plasticizer
Evonik VESTINOL® 9 Plasticizer
Evonik Modifier OH 650 Plasticizer
Evonik Modifier 715 Plasticizer
Eastman Benzoflex™ PS-507 Plasticizer

PEVONIL984 / 197188

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.