MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

CRP  Windform

(Viewing data as-entered. Click here to return)
Mitsubishi FGF Recycled ASA-X 20% Glassfibe ASA, 30% Glass Fiber Filled 3D Printing Polymer
Categories: Polymer; 3D Printing/Additive Manufacturing Polymer; Renewable/Recycled Polymer; Thermoplastic; ASA Polymer; Acrylonitrile/Styrene/Acrylate (ASA), 15% Glass Reinforced

Material Notes: FGF Recycled ASA-X 20% Glass fiber is a specially developed modified ASA compound, made from Mitsubishi's own industrial waste to ensure the quality of the product. The low warpage ASA compound with added glass fibers gives great features which work well with a variety of applications

Features:

  • 20% filled with Glass fiber
  • Low warpage
  • Easy to print
  • UV resistant
  • Good layer adhesion
Colors on request.

Information provided by Mitsubishi Chemical.

Vendors: Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.27 g/ccISO 1183
Melt Flow 16 g/10 min
@Load 10.0 kg,
Temperature 220 °C
ISO 1133
Storage Temperature 15.0 - 25.0 °C
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break 81.0 MPaISO 527
Tensile Strength, Yield 81.0 MPaISO 527
Elongation at Break 2.4 %ISO 527
Elongation at Yield 2.2 %ISO 527
Tensile Modulus 6300 MPaISO 527
Charpy Impact, Notched 6.20 kJ/m²ISO 179
 
Thermal PropertiesOriginal ValueComments
Vicat Softening Point 85.0 °CISO 306 B
 
Processing PropertiesOriginal ValueComments
Zone 1 200 - 240 °C
Zone 2 200 - 240 °C
Zone 3 200 - 240 °C
Die Temperature 210 - 250 °C
Drying Temperature 75.0 °C<250 ppm
Dry Time 4.00 hour
 
Descriptive Properties
Mass Temperature220°C

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PMITS9817 / 301042

Ensinger PEI

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.