MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Celanese Zytel® HTNFR52G45NHF BK337 PA6T/66-GF45FR(40)
Categories: Polymer; Thermoplastic; Polyphthalamide (PPA); Polyphthalamide (PPA), 50% Glass Fiber Reinforced

Material Notes: 45% Glass Reinforced, Flame Retardant, Non-Halogenated, PPA, High Performance Polyamide

Former DuPont product acquired by Celanese in 2022.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.61 g/ccDAM; ISO 1183
Linear Mold Shrinkage, Flow 0.0020 cm/cmDAM; ISO 294-4, 2577
Linear Mold Shrinkage, Transverse 0.0060 cm/cmDAM; ISO 294-4, 2577
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break 174 MPaDAM; ISO 527-1/-2
Elongation at Break 1.8 %DAM; ISO 527-1/-2
Tensile Modulus 15700 MPaDAM; ISO 527-1/-2
Flexural Strength 255 MPaDAM; ISO 178
Flexural Modulus 15600 MPaDAM; ISO 178
Poissons Ratio 0.33DAM
Charpy Impact Unnotched 45.0 kJ/m²
@Temperature -30.0 °C
DAM; ISO 179/1eU
 47.0 kJ/m²
@Temperature 23.0 °C
DAM; ISO 179/1eU
Charpy Impact, Notched 8.00 kJ/m²
@Temperature -30.0 °C
DAM; ISO 179/1eA
 8.00 kJ/m²
@Temperature 23.0 °C
DAM; ISO 179/1eA
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity >= 1.00e+15 ohm-cmDAM; IEC 62631-3-1
 
Thermal PropertiesOriginal ValueComments
CTE, linear, Parallel to Flow 17.0 µm/m-°CDAM; ISO 11359-1/-2
 15.0 µm/m-°C
@Temperature -40.0 - 23.0 °C
DAM; ISO 11359-1/-2
 15.0 µm/m-°C
@Temperature 55.0 - 160 °C
DAM; ISO 11359-1/-2
CTE, linear, Transverse to Flow 55.0 µm/m-°CDAM; ISO 11359-1/-2
 50.0 µm/m-°C
@Temperature -40.0 - 23.0 °C
DAM; ISO 11359-1/-2
 95.0 µm/m-°C
@Temperature 55.0 - 160 °C
DAM; ISO 11359-1/-2
Melting Point 310 °Cfirst heat; DAM; ISO 11357-1/-3
Deflection Temperature at 1.8 MPa (264 psi) 283 °CDAM; ISO 75-1/-2
Glass Transition Temp, Tg 45.0 °C10°C/min; 50% RH; ISO 11357-1/-2
 90.0 °C10°C/min; DAM; ISO 11357-1/-2
UL RTI, Electrical 140 °C
@Thickness 0.400 mm
UL 746B
 140 °C
@Thickness 0.750 mm
UL 746B
 140 °C
@Thickness 1.50 mm
UL 746B
 140 °C
@Thickness 3.00 mm
UL 746B
Flammability, UL94 V-0
@Thickness 0.400 mm
DAM; IEC 60695-11-10
 
Processing PropertiesOriginal ValueComments
Melt Temperature 320 - 325 °CRange, Injection
Mold Temperature 90.0 - 130 °CInjection
Drying Temperature 100 °CInjection
Dry Time 6.00 - 8.00 hourInjection, Dehumidified Dryer
Moisture Content <= 0.10 %Injection
 
Descriptive Properties
AdditivesFlame retardant
 Non-halogenated/Red phosphorous free flame retardant
Drying RecommendedyesInjection
ISO designationISO 16396-PA6T/66,GF45 FR(40),M1CF1G,S10-160
Part Marking Code>PA6T/66-GF45FR(40)<ISO 11469
 >PPA-GF45FR<SAE J1344
PolymerPA6T/66-GF45 FR(40)
Resin IdentificationPA6T/66-GF45FR(40)ISO 1043

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PDSX5466a / 291027

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.