Description: - One of the BioBlend® XP family of high performance BioPolymers designed for blown film applications.
- BioBlend® XP 24850 is a masterbatch that contains 50% NuPlastiQ GP BioPolymer compounded with octene LLDPE.
- Made from 50% annually renewable agricultural resources.
- Supplied in pellet form.
Applications: - Used for final products requiring strength and plasticity, such as packaging.
Information provided by |