MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

(Viewing data as-entered. Click here to return)
BJB Enterprises F-140 REV 1 A/B Polyurethane Elastomer
Categories: Polymer; Thermoset; Polyurethane, TS; Thermoset Polyurethane, Elastomer, Unreinforced

Material Notes: The F-1 Series addresses the need for shorter processing times and higher part production. These products exhibit excellent physical properties and easily process at room temperature. The easy mix ratio is extremely convenient and cartridge dispense friendly.

Features: RoHS/REACH Compliant, Roto-Cast Parts, High Tensile & Tear Strength, Special Effects & Props, Over Molding, Easy to Pigment.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.018 g/cc
@Temperature 25.0 °C
Part B
 1.046 g/cc
@Temperature 25.0 °C
Part A
Density 1.056 g/ccASTM D792-00
Brookfield Viscosity 1000 cP
@Temperature 25.0 °C
Part B
 1100 cP
@Temperature 25.0 °C
Mixed Part A & Part B
 1150 cP
@Temperature 25.0 °C
Part A
Storage Temperature 65.0 - 80.0 °F
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore A 35 - 45ASTM D2240-04e1
Tensile Strength 940 psiASTM D412-98a(2002)e1
Elongation at Break 800 %ASTM D412-98a(2002)e1
Tensile Modulus 180 psiASTM D412-98a(2002)e1
Tear Strength 120 pliASTM D624-00e1
 
Electrical PropertiesOriginal ValueComments
Dielectric Constant 5.661
@Frequency 1e+6 Hz
ASTM D150-87
Dissipation Factor 0.0618
@Frequency 1e+6 Hz
ASTM D150-87
 
Processing PropertiesOriginal ValueComments
Processing Temperature <= 200 °FMax cure temp.
Cure Time 1.00 - 3.00 hour
@Temperature 25.0 °C
Step 1 recommended high temp cure (as tested).
 16.0 hour
@Temperature 71.1 °C
Step 2 recommended high temp cure (as tested).
 120 - 168 hour
@Temperature 25.0 °C
Optional low temp cure
Working Life 7.00 - 8.00 min
@Temperature 25.0 °C
100 g.
Gel Time 9.00 - 10.0 min
Shelf Life 6.00 MonthStored at recommended temperatures. Purge opened containers with dry nitrogen before resealing.
 
Descriptive Properties
Color / AppearanceAmberPart B
 Pale YellowPart A
 Translucent AmberCured
Demold Time (hrs)3 - 4@ 77°F
Mix Ratio by volume49 to 100Part A to Part B. (cartridge dispense friendly)
Mix Ratio by weight50 to 100Part A to Part B

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PBJB9915 / 287695

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.