MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Qualchem Danamid FEWLX2-25 Polyamide 6, 25% Mineral Filled
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 6 (PA6)

Material Notes: Filled with minerals. Flame retardant, halogen-free (V-2)

Information provided by Qualchem Zrt.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.42 g/ccDIN 53479
Filler Content 23 - 27 %
Moisture Absorption at Equilibrium 2.0 - 2.2 %DIN 53714
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break 48.0 MPa50 mm/min; ISO 527-1,2
Elongation at Break 4.0 %ISO 527-1,2
Tensile Modulus 2.70 GPaISO 527-1,2
Izod Impact, Notched (ISO) 3.40 kJ/m²
@Temperature 23.0 °C
ISO 180
Izod Impact, Unnotched (ISO) 15.0 kJ/m²ISO 180
Charpy Impact Unnotched 1.90 J/cm²
@Temperature 23.0 °C
DIN 53453
 1.90 J/cm²
@Temperature -30.0 °C
DIN 53453
Charpy Impact, Notched 0.330 J/cm²
@Temperature 23.0 °C
DIN 53453
 0.330 J/cm²
@Temperature -30.0 °C
DIN 53453
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 1.00e+14 ohm-cmDIN 53482
Comparative Tracking Index 450 VIEC 112
 
Thermal PropertiesOriginal ValueComments
Flammability, UL94 V-2
@Thickness 4.00 mm
MSZ 10383
Glow Wire Test 960 °C
@Thickness 3.50 mm
IEC 685-2-1

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PQUALC30 / 58442

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.