Function: Curing activator for chloroprene (CR) and butyl (IIR) rubber as well as chlorosulfonated polyethylene (CSM). Filler in compounds for protective covering owing to high capacity to absorb X-rays. Application: Water resistant rubber articles; activation of the vulcanization of butyl and chloroprene rubbers; X-ray articles, e. g. gloves, aprons Information provided by Lanxess. |