Property data below is typical of annealed samples. Available in sheet, strip and plate. Intended for high-strength non-magnetic applications and aircraft parts such as hydraulic tubing. Information provided by Allegheny Ludlum |
DIN 1.4454; ASTM A-666; AMS 5595 |