MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
NanoScale NanoActive® Titanium Dioxide  (discontinued **)
Categories: Ceramic; Oxide; Titanium Oxide

Material Notes: NanoActive TiO2 is produced using proprietary processes to obtain high specific surface area (over 500 m²/g), high porosity, weakly aggregated, amorphous material possessing adsorption capacity and chemical reactivity.

Applications: Applications include catalysts and catalyst supports, cosmetic and skin care market, destruction of chemical warfare agents, paints and coatings, protective apparel and personal protection equipment, smoke removal, structural ceramics, and UV protecting clear coats.

Information provided by NanoScale

Composition based on metal

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Bulk Density 0.600 g/cc
Density 3.70 g/cc
Moisture Absorption <= 4.0 %
Loss On Ignition <= 12 %
Particle Size 5.0 µmmean aggregate size
Specific Surface Area >= 500 m²/gBET
Pore Size 0.00320 micronsAverage Diameter
 
Component Elements PropertiesOriginal ValueComments
Titanium, Ti >= 99.999 %
 
Descriptive Properties
Appearance / ColorWhite Powder
Crystallite SizeAmorphous
Minimum Total Pore Volume cc/g0.4

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Titanium Dioxide, Rutile
Titanium Dioxide, TiO2, Anatase
Titanium Dioxide, Brookite
Lanxess PUROLAN® E 171 A Pharma Phamaceutical Grade Titanium Dioxide TiO2
DSM Biomedical PurSil® 20 Thermoplastic Silicone Polyether Polyurethane (TSPU)

CNANO07 / 1669

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.