MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Crosspolimeri GETILAN ATP/190 3AP Crosslinkable Polyolefinic
Categories: Polymer; Thermoplastic; Polyolefin

Material Notes: GETILAN: is the trade-mark of our crosslinkabe (SIOPLAS technology) polyolefinic compounds

GETILAN ATP/190 3AP: high density antiflame chemically crosslinkable polythene with high temperature index and low HCl content. Suitable for automotive cables insulation. It is a conveniently grafted polythene able to react in presence of moisture and of catalyst. We normally suggest our catalysts type MAC/203 HS or MAC/203 HSL (less reactive). REACTION BETWEEN GRAFTING AND CATALYST: These two polythene, separately stored, must be mixed before starting extrusion in the ratio: GRAFTING/CATALYST 96/4

Certify: SAE J1127/J1128, FIAT 7.Z8220 T3 -T3 S, ISO 6722 -LV 112 Class C

Information provided by Crosspolimeri S.P.A.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.15 g/ccISO R 118.3
Melt Flow 18 - 25 g/10 min
@Load 21.6 kg,
Temperature 190 °C
ASTM D1238
Storage Temperature 12.0 °C
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore D 59ASTM D2240
Tensile Strength >= 14.0 MPaASTM D638
Elongation at Break >= 200 %ASTM D638
 
Processing PropertiesOriginal ValueComments
Zone 1 130 °C
Zone 2 145 °C
Zone 3 175 °C
Zone 4 185 °C
Die Temperature 200 - 210 °C
Head Temperature 190 - 195 °C
 
Descriptive Properties
Exercise temperature- 40 + 125°C
Halogen Content<12%IEC 754-1
Hot Set Test<5%Residual Value, IEC 60811
 0.5200°C - 20 N/cm2, IEC 60811

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PCROS111 / 294195

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.