MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
LNP Cycolac® SLA5891 Acrylonitrile Butadiene Styrene  (discontinued **)
Categories: Polymer; Thermoplastic; ABS Polymer; Acrylonitrile Butadiene Styrene (ABS), Molded

Material Notes: Transparent based resin: to provide a good balance between clarity, impact resistance and processability. Will become CSD5100T.

  • Features: Good Processability, High Clarity, Good Impact Resistance, Antistatic
  • Forms: Pellets
  • Processing Method: Injection Molding
Information provided by LNP, a GE Plastics Company.

This data sheet is labeled Discontinued; however many LNP grades are still active under new names instituted after the SABIC purchase.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.09 g/ccASTM D792
Linear Mold Shrinkage 0.0045 - 0.0065 cm/cm
@Thickness 3.18 mm
ASTM D955
Melt Flow 13 g/10 min
@Load 3.80 kg,
Temperature 230 °C
ASTM D1238
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break 29.6 MPaType I, 5 mm/min; ASTM D638
Tensile Strength, Yield 36.5 MPaType I, 5 mm/min; ASTM D638
Elongation at Break 27 %Type I, 5 mm/min; ASTM D638
Flexural Yield Strength 56.5 MPa(50.8 mm Span) 1mm/min; ASTM D790
Flexural Modulus 1.87 GPa(50.8 mm Span) 1mm/min; ASTM D790
Izod Impact, Notched 1.07 J/cmASTM D256
Falling Dart Impact 35.9 JASTM D3763
 
Electrical PropertiesOriginal ValueComments
Surface Resistance 2.00e+12 ohmASTM D257
Static Decay <= 1.5 sec5000V to <50V; FTMS101B
 
Thermal PropertiesOriginal ValueComments
Deflection Temperature at 1.8 MPa (264 psi) 68.3 °C
@Thickness 3.18 mm
Unannealed; ASTM D648
 
Optical PropertiesOriginal ValueComments
Transmission, Visible 85 %Transparent, but thickness unknown
 
Processing PropertiesOriginal ValueComments
Rear Barrel Temperature 188 - 210 °C
Middle Barrel Temperature 204 - 218 °C
Front Barrel Temperature 216 - 227 °C
Nozzle Temperature 218 - 238 °C
Melt Temperature 218 - 238 °C
Mold Temperature 48.9 - 71.1 °C
Drying Temperature 71.1 - 76.7 °C
Dry Time 2 - 8 hour
Moisture Content 0.010 %Suggested
Back Pressure 0.345 - 0.689 MPa
Shot Size 50 - 70 %Suggested
Vent Depth 0.00380 - 0.00510 cm
Screw Speed 30 - 60 rpm

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
LNP Cycolac® EXCP0057 Acrylonitrile Butadiene Styrene
LNP Cycolac® EXCP0153 Acrylonitrile Butadiene Styrene
LNP Cycolac® 29438A Acrylonitrile Butadiene Styrene
LNP Cycolac® SLA5853 Acrylonitrile Butadiene Styrene
LNP Cycolac® SLA5850 Acrylonitrile Butadiene Styrene, 5.0 % PTFE Lubricant

PZLNP1009 / 51091

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.