MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Toyobo GLAMIDE® TY-102ND Nylon/Elastomer
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA)

Material Notes: GLAMIDE® is very tough and exhibits high abrasion resistance. It has a high melting point and heat resistance, has well-balanced proportions of mechanical properties, performs self-distinguishing and a specific grade approved as UL94V-0 class is provided, and it exhibits excellent chemical resistance and oil resistance. Grade TY-102ND is a super tough, non-reinforced alloy of nylon and elastomer.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.09 g/ccAbsolute Drying; ASTM-D792
Water Absorption 1.0 %Absolute Drying; ASTM-D570
Moisture Absorption at Equilibrium 2.9 %Absolute Drying; ASTM-D570
Linear Mold Shrinkage 0.0070 - 0.010 cm/cm
@Thickness 1.00 mm
Absolute Drying
 0.015 - 0.020 cm/cm
@Thickness 3.00 mm
Absolute Drying
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell R 102Absolute Drying; ASTM-D785
Tensile Strength, Ultimate 15.0 MPa
@Temperature 80.0 °C
Practical Use (Water Absorption 2.9%); ASTM-D638
 21.0 MPa
@Temperature 80.0 °C
Absolute Drying; ASTM-D638
 27.0 MPa
@Temperature 23.0 °C
Practical Use (Water Absorption 2.9%); ASTM-D638
 50.0 MPa
@Temperature 23.0 °C
Absolute Drying; ASTM-D638
 74.0 MPa
@Temperature -40.0 °C
Practical Use (Water Absorption 2.9%); ASTM-D638
 85.0 MPa
@Temperature -40.0 °C
Absolute Drying; ASTM-D638
Elongation at Break >= 200 %ASTM-D638
Flexural Strength 17.0 MPa
@Temperature 80.0 °C
Practical Use (Water Absorption 2.9%); ASTM-D790
 27.0 MPa
@Temperature 80.0 °C
Absolute Drying; ASTM-D790
 35.0 MPa
@Temperature 23.0 °C
Practical Use (Water Absorption 2.9%); ASTM-D790
 75.0 MPa
@Temperature 23.0 °C
Absolute Drying; ASTM-D790
 87.0 MPa
@Temperature -40.0 °C
Practical Use (Water Absorption 2.9%); ASTM-D790
 94.0 MPa
@Temperature -40.0 °C
Absolute Drying; ASTM-D790
Flexural Modulus 0.200 GPa
@Temperature 80.0 °C
Practical Use (Water Absorption 2.9%); ASTM-D790
 0.600 GPa
@Temperature 80.0 °C
Absolute Drying; ASTM-D790
 0.800 GPa
@Temperature 23.0 °C
Practical Use (Water Absorption 2.9%); ASTM-D790
 2.00 GPa
@Temperature 23.0 °C
Absolute Drying; ASTM-D790
 2.30 GPa
@Temperature -40.0 °C
Practical Use (Water Absorption 2.9%); ASTM-D790
 2.70 GPa
@Temperature -40.0 °C
Absolute Drying; ASTM-D790
Izod Impact, Notched 150 J/m
@Temperature -40.0 °C
Absolute Drying; ASTM-D256
 180 J/m
@Temperature -40.0 °C
Practical Use (Water Absorption 2.9%); ASTM-D256
 310 J/m
@Temperature 23.0 °C
Absolute Drying; ASTM-D256
 NB
@Temperature 23.0 °C
Practical Use (Water Absorption 2.9%); ASTM-D256
Taber Abrasion, mg/1000 Cycles 8.0CS-17, Absolute Drying; ASTM-D1044
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 1.00e+9 ohm-cmPractical Use (Water Absorption 2.9%); ASTM-D257
 1.00e+12 ohm-cmAbsolute Drying; ASTM-D257
Dielectric Strength 14.0 kV/mm
@Thickness 2.00 mm
Practical Use (Water Absorption 2.9%); ASTM-D149
 18.0 kV/mm
@Thickness 2.00 mm
Absolute Drying; ASTM-D149
Arc Resistance 108 secPractical Use (Water Absorption 2.9%); ASTM-D495
 125 secAbsolute Drying; ASTM-D495
Comparative Tracking Index >= 600 VIEC Method
 
Thermal PropertiesOriginal ValueComments
CTE, linear 87.0 µm/m-°CAbsolute Drying; ASTM-D696
Deflection Temperature at 0.46 MPa (66 psi) 150 °CAbsolute Drying; ASTM-D648
Deflection Temperature at 1.8 MPa (264 psi) 58.0 °CAbsolute Drying; ASTM-D648
Flammability, UL94 HB
 
Processing PropertiesOriginal ValueComments
Melt Temperature 245 - 285 °C
Mold Temperature 50.0 - 80.0 °C
Injection Pressure 40.0 - 80.0 MPa

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Multibase Multi-Flex® TPO D-6500
Multibase Multi-Flex® TPO D-6206

PTOY920 / 107471

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.