MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

(Viewing data as-entered. Click here to return)
Nouryon Armostat 600 (Hydrogenated tallow)-bis(2-hydroxyethyl) amine
Categories: Other Engineering Material

Material Notes: Hydrogenated tallow-based antistat typically used in BOPP and PP. Provides sustained antistatic properties and shows excellent thermal stability due to its saturated alkyl chain, making it especially suitable for applications needing higher processing temperatures.

Applications: Armostat 600 is a tallow based saturated alkylbis(2-hydroxyethyl) amine. Armostat 600 is an internal antistatic additive that can be used in various polymers such as PE, LLDPE, PP, SAN and ABS. Armostat 600 gives sustained antistatic action and shows excellent thermal stability due to its saturated alkyl chain. This makes Armostat 600 especially suitable for those applications needing higher processing temperatures. Armostat 600 is a solid at ambient temperatures. When heated at 50-55°C the product can be dosed as a liquid directly into the polymer by using a single or twin-screw extruder. Pigment or color concentrates should be mixed with the antistatic agent prior to extruding. Premixing ensures uniform distribution of Armostat 600 in the resin while Armostat 600 acts as a dispersion aid to the pigment color concentrate.

CAS number: 90367-28-5

EINECS/ELINCS No.: 291-276-3

Information provided by Nouryon

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.910 g/cc
@Temperature 25.0 °C
 0.960 g/cc
@Temperature 20.0 °C
Viscosity 150 cP
Vapor Pressure <= 0.000100 bar
 
Thermal PropertiesOriginal ValueComments
Flash Point 219 °CCleveland open cup
 
Component Elements PropertiesOriginal ValueComments
H2O, Water <= 0.20 %
 
Descriptive Properties
AppearanceSlightly yellowish solid
Clear point44 °C
Color= 150 Pt-Co
Content= 97.0 %Tertiary amine content
Equivalent weight338-360 g/eq

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PNOURY270 / 285793

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.