MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Trinseo CALIBRE™ 703-15 Polycarbonate Resin  (discontinued **)
Categories: Polymer; Thermoplastic; Polycarbonate (PC)

Material Notes: Overview: CALIBRE™ 701-15 Series resins are formulated and produced to supply both clarity and enhanced ignition resistance. They do so while maintaining excellent physical properties and processability. The CLIBRE 701-15 series products are available in 2 additive packages: CLIBRE 701: Mold release. CALIBRE 7003: Mold release and UV stabilizer.

Main Characteristics:

  • Underwriters Laboratory Inc. (UL)
Applications:
  • Industrial switches
  • Circuit breakers
  • Plugs, sockets and switches
  • Street lights
  • Safety lights
  • Reflectors

Information provided by Styron

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.20 g/ccISO 1183/A
Linear Mold Shrinkage, Flow 0.0050 - 0.0070 in/inISO 294-4
Melt Flow 15 g/10 min
@Load 1.20 kg,
Temperature 300 °C
ISO 1133
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break 66.0 MPaISO 527-2/50
Tensile Strength, Yield 60.0 MPaISO 527-2/50
Elongation at Break 120 %ISO 527-2/50
Elongation at Yield 6.0 %ISO 527-2/50
Tensile Modulus 2300 MPaISO 527-2/50
Flexural Strength 100 MPa2.0 mm/min (3 point); ISO 178
Flexural Modulus 2400 MPa2.0 mm/min (3 point); ISO 178
Izod Impact, Notched (ISO) 83.0 kJ/m²
@Temperature 23.0 °C
ISO 180/A
Charpy Impact, Notched 20.0 kJ/m²
@Temperature 23.0 °C
ISO 179/1eA
 
Electrical PropertiesOriginal ValueComments
Comparative Tracking Index 250 V
@Thickness 2.00 mm
Solution A; IEC 60112
 
Thermal PropertiesOriginal ValueComments
Hot Ball Pressure Test 125 °CIEC 60335-1
Deflection Temperature at 0.46 MPa (66 psi) 142 °CAnnealed; ISO 75-2/B
Deflection Temperature at 1.8 MPa (264 psi) 122 °CUnannealed; ISO 75-2/A
 139 °CAnnealed; ISO 75-2/A
Vicat Softening Point 147 °CISO 306/B50
Flammability, UL94 V-2
@Thickness 1.60 mm
 V-0
@Thickness 3.20 mm

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Trinseo CALIBRE™ 603-3 Polycarbonate, Branched

PZZDWST025 / 142234

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.