MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
3M FireDam™ 200 Spray
Categories: Polymer; Thermoset; Rubber or Thermoset Elastomer (TSE)

Material Notes: 3M Fire Dam Spray 200 is a sprayable water-based material that dries to form a tough, elastomeric coating. This material is used to firestop perimeter joints (curtain wall), construction joints and through penetration openings. When installed properly, will help control the transmission of fire, heat, and smoke before, during, and after exposure to fire.

Information provided by 3M

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Volatiles 35 %
Viscosity 120000 cPwith shear thinning
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore A >= 60ASTM D2240
 
Processing PropertiesOriginal ValueComments
Shelf Life >= 4.00 Month
 
Descriptive Properties
AppearanceGray or Red

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
SYNTHOS Kralex® 1712 Styrene Butadiene Rubber
SYNTHOS Kralex® 1706 Styrene Butadiene Rubber
Overview of materials for Thermoset Fluoroelastomer
Overview of materials for High Density Polyethylene (HDPE), Injection Molded
Overview of materials for Acrylonitrile Butadiene Styrene (ABS), Extruded

PMM35446 / 170193

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.