MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Evonik Polymer RV 200
Categories: Polymer

Material Notes: Products of the Polymer XP RV range are vinyl-functional polydimethyl siloxanes of various molecular weights. They contain both, terminal and pendant vinyl groups. Due to this structure, they produce higher crosslinking densities than Polymer VS at similar viscosity levels.

Application: Polymer XP RV can be used as a base polymer or as an additive with Polymer VS. It cures by a platinum-catalyzed addition reaction with silicone crosslinkers containing SiH-groups. The formulator can adjust the formulation properties over a wide range by selecting the suitable crosslinkers (Crosslinker 100 series, Crosslinker 200 series), catalysts (Catalyst 500 series), additives and fillers (VQM, Compound VS).

Information provided by Evonik

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.00 g/cc
Viscosity 360 cP
 
Optical PropertiesOriginal ValueComments
Refractive Index 1.413
 
Descriptive Properties
Appearanceclear, colorless liquid
Content2.3%Vinyl

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Evonik Polymer RV 5000
Evonik Polymer RV 100

PEVONIM090 / 197294

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.