MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

(Viewing data as-entered. Click here to return)
BASF Ultramid® A 218 V25 Black 21N Nylon 66, 25% Glass Fiber Reinforced, Heat Stabilized, Dry
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 66 (PA66); Nylon 66, 30% Glass Fiber Filled; Nylon 66, Heat Stabilized

Material Notes: Product Description: Ultramid® A 218 V25 Black 21N is a polyamide 66, reinforced with 25% of glass fiber, heat stabilized, for injection molding. This grade offers an excellent combination between thermal and mechanical properties.

Availability: Africa & Middle East; Asia Pacific; Latin America; North America

Filler/Reinforcement: Glass Fiber, 25% Filler by Weight

Additive: Heat Stabilizer

Features: Good Flow; Good Mold Release; Heat Stabilized - Inorganic

Use: Automotive Applications; Consumer Applications; Handles; Industrial Applications

Agency Ratings: EC 1907/2006 (REACH)

RoSH Compliance: RoSH Compliant

Appearance: Black; Natural Color

Forms: Pellets

Processing Method: Injection Molding

Resin ID (ISO 1043): PA66-GF25

Information provided by BASF Corporation

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.32 g/ccISO 1183
Water Absorption 2.3 %Equilibrium, 50% RH; ISO 62
 0.90 %
@Time 86400 sec
ISO 62
Water Absorption at Saturation 6.2 %ISO 62
Maximum Moisture Content 0.20
Linear Mold Shrinkage, Flow 0.011 cm/cmISO 294-4
Linear Mold Shrinkage, Transverse 0.0040 cm/cmISO 294-4
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break 23200 psiASTM D638
 23900 psiISO 527-2
Elongation at Break 3.0 %ISO 527-2
 3.3 %ASTM D638
Tensile Modulus 1.22e+6 psiISO 527-1
Flexural Strength 34800 psiISO 178
 36300 psiASTM D790
Flexural Modulus 1.06e+6 psiISO 178
 1.06e+6 psiASTM D790
Izod Impact, Notched 1.50 ft-lb/inASTM D256
Izod Impact, Notched (ISO) 4.00 ft-lb/in²ISO 180/A
Izod Impact, Unnotched (ISO) 26.0 ft-lb/in²ISO 180
Charpy Impact Unnotched 28.0 ft-lb/in²ISO 179/1eU
Charpy Impact, Notched 4.80 ft-lb/in²ISO 179/1eA
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 1.00e+15 ohm-cmIEC 62631-3-1
Dielectric Constant 3.7
@Frequency 100 Hz
IEC 62631-2-1
Dielectric Strength 810 V/mil
@Thickness 2.00 mm
IEC 60243-1
Dissipation Factor 0.010
@Frequency 100 Hz
IEC 62631-2-1
Comparative Tracking Index 400 VSolution A; IEC 60112
 
Thermal PropertiesOriginal ValueComments
Melting Point 504 °FISO 11357-3
Deflection Temperature at 1.8 MPa (264 psi) 473 °FUnannealed; ASTM D648
 482 °FUnannealed; ISO 75-2/A
Flammability, UL94 HB
@Thickness 0.762 mm
IEC 60695-11-10,-20
 HB
@Thickness 1.52 mm
IEC 60695-11-10,-20
Oxygen Index 23 %ISO 4589-2
Glow Wire Flammability Index 1200 °F
@Thickness 1.52 mm
IEC 60695-2-12
 
Processing PropertiesOriginal ValueComments
Rear Barrel Temperature 518 - 536 °F
Middle Barrel Temperature 527 - 545 °F
Front Barrel Temperature 536 - 554 °F
Mold Temperature 158 - 212 °F
Drying Temperature 176 °F

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PBASG2104 / 310797

Ensinger PEI

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.