MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Proto3000 316L MIM - MPIF 35 Stainless Steel; As-Sintered
Categories: Metal; 3D Printing/Additive Manufacturing Metal; Ferrous Metal; Stainless Steel; T 300 Series Stainless Steel

Material Notes: 316L is a molybdenum-bearing, fully-austenitic 3D Printed Stainless steel. It’s known for its excellent corrosion resistance and mechanical properties at both high and low temperatures.

Applications: 316L 3D Printed Stainless steel is a common material used in many applications, such as chemical and petrochemical processing, food processing, laboratory equipment, medical devices, marine, jewelry, power generation, petroleum refining, water treatment, pulp and paper manufacturing.

  • Marine
  • Power Generation
  • Jewelry
  • Petroleum Refining
  • Food Processing
  • Laboratory Equipment
  • Chemical and Petrochemical Processing
  • Medical Devices
  • Pulp and Paper Manufacturing

Property data per MPIF Standard 35.

Information provided by Proto3000

Key Words: UNS S31673, EN 1.4404
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density >= 7.60 g/cc
Porosity <= 5.00 %
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell B 67.0ASTM E18
Tensile Strength, Ultimate >= 450 MPaASTM E8M
Tensile Strength, Yield >= 140 MPaASTM E8M
Elongation at Break >= 40.0 %ASTM E8M
 
Component Elements PropertiesOriginal ValueComments
Carbon, C <= 0.0300 %
Chromium, Cr 16.0 - 18.0 %
Iron, Fe 61.97 - 72.0 %Balance
Manganese, Mn <= 2.00 %
Molybdenum, Mo 2.00 - 3.00 %
Nickel, Ni 10.0 - 14.0 %
Silicon, Si <= 1.00 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

NPROTO884 / 322897

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.