MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Refractory Metals

(Viewing data as-entered. Click here to return)
Tantalum, Ta; Annealed
Categories: Metal; Nonferrous Metal; Refractory Metal; Pure Element

Material Notes: Annealed applies only to tensile and/or hardness values; other property values are typical of the element.

Vendors: Eagle Alloys Corporation is a leading supplier of quality metals and alloys. Our staff prides itself on working fast, efficiently and courteously to get you the information you need. Call (800) 237-9012 or visit www.EagleAlloys.com.

PLANSEE SE: Whether it's high temperatures, aggressive chemicals or extreme mechanical loading: PLANSEE supplies a suitable product solution in refractory metals or composite materials. As the world market leader in powder metallurgically produced high performance materials we combine outstanding materials knowledge with profound applications and technology know-how. Visit us at www.plansee.com.

Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesOriginal ValueComments
Density 16.65 g/cc
Vapor Pressure 6.298e-9 bar
@Temperature 2351 °C
 7.488e-9 bar
@Temperature 2365 °C
 4.019e-8 bar
@Temperature 2487 °C
 9.82e-8 bar
@Temperature 2566 °C
 1.72e-7 bar
@Temperature 2615 °C
 2.44e-7 bar
@Temperature 2652 °C
 3.703e-7 bar
@Temperature 2675 °C
 
Chemical PropertiesOriginal ValueComments
Atomic Mass 180.94791995
Atomic Number 73
Thermal Neutron Cross Section 21.3 barns/atom
X-ray Absorption Edge 0.18393 ÅK
 1.06084 ÅLI
 1.11264 ÅLII
 1.25427 ÅLIII
Electrode Potential 4.1 V
Electronegativity 1.5Pauling
Ionic Radius 0.680 ÅCrystal Ionic Radius for Valence +5
 
Mechanical PropertiesOriginal ValueComments
Hardness, Brinell 95Converted from Vickers for 3000 kg load/10 mm ball Brinell test.
Hardness, Rockwell A 35Converted from Vickers.
Hardness, Rockwell B 51Converted from Vickers.
Hardness, Vickers 100
Tensile Strength, Ultimate 450 MPa
Modulus of Elasticity 186 GPa
Poissons Ratio 0.35
Fatigue Strength 230 MPa
@# of Cycles 5.00e+7
E-beam melted sample; rotating beam test.
Shear Modulus 69.0 GPa
 
Electrical PropertiesOriginal ValueComments
Electrical Resistivity 0.0000125 ohm-cm
Magnetic Susceptibility 9.0e-7cgs/g
Critical Magnetic Field Strength, Oersted 823 - 835
Critical Superconducting Temperature 4.43 - 4.51 K
 
Thermal PropertiesOriginal ValueComments
Heat of Fusion 170 J/g
CTE, linear 6.50 µm/m-°C
@Temperature 20.0 °C
 6.60 µm/m-°C
@Temperature 250 °C
 6.70 µm/m-°C
@Temperature 500 °C
 6.96 µm/m-°C
@Temperature 1000 °C
Specific Heat Capacity 0.153 J/g-°C
Thermal Conductivity 54.4 W/m-K
@Temperature 20.0 °C
 56.1 W/m-K
@Temperature -73.0 °C
 59.9 W/m-K
@Temperature 127 °C
 66.6 W/m-K
@Temperature 527 °C
 72.9 W/m-K
@Temperature 927 °C
 77.0 W/m-K
@Temperature 1327 °C
 80.8 W/m-K
@Temperature 1727 °C
 83.7 W/m-K
@Temperature 2127 °C
 85.8 W/m-K
@Temperature 2527 °C
Melting Point 2996 °C
Boiling Point 5458 °C
 
Optical PropertiesOriginal ValueComments
Emissivity (0-1) 0.49650 nm
 0.20
@Temperature 1460 °C
Total Hemispherical
 
Component Elements PropertiesOriginal ValueComments
Tantalum, Ta 100 %
 
Descriptive Properties
CAS Number7440-22-7

References for this datasheet.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Tantalum, Ta; Cold Worked
Tantalum, UNS R05200
Tantalum, UNS R05400
Tungsten, W
Molybdenum, Mo, Annealed

AMETa01 / 107

Free Trade Publications, Click Here!
Free Trade Publications, Click Here!

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.