Description: LINXIDAN® LX4530 is a polyolefin plastomer with a silane copolymer functionality, designed to improve compatibility and mechanical properties of polymer compounds. Contrarily to conventionally maleated polyolefin coupling agents, LINXIDAN® LX4530 does not interfere with metal stearates used as lubricants in Wood Plastics Composites (WPC), providing increased tensile strength, impact strength and flexural modulus, and reduced moisture absorption..Information provided by SACO AEI Polymers. |