MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Chesterton ARC S1PW Ceramic-Filled Epoxy Industrial Coating
Categories: Polymer; Thermoset; Epoxy

Material Notes: 100% solids, reinforced thin film coating to protect structures against chemical, erosion and corrosion attack. ARC S1PW is certified for cold water service requiring NSF 61 certification. ARC S1PW is designed to: Provide excellent barrier protection against erosion, corrosion and chemical attack; Meet all requirements of NSF 61 for potable, cold water service; Easily apply by brush, roller or plural component spray

Filler: Blend of fine aluminum oxide powders & micro glass flakes treated with polymeric coupling agent. Matrix: A modified epoxy resin reacted with polyamidoamine curing agent

Information provided by Chesterton

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.59 g/ccCured
Solids Content 100 %
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore D 87ASTM D2240
Elongation at Break 3.15 %ASTM D638
Flexural Strength 9520 psiASTM D790
Flexural Modulus 540000 psiASTM C580
Compressive Strength 10180 psiASTM D695
Adhesive Bond Strength 6790 psiPull-Off Adhesion vs. Metal; ASTM D4541
 
Thermal PropertiesOriginal ValueComments
Maximum Service Temperature, Air 23.0 °CWet Service per NSF 61
 52.0 °CWet Service
 62.0 °CDry Service
 
Processing PropertiesOriginal ValueComments
Shelf Life 12.0 Month
@Temperature 10.0 - 32.0 °C
Dry, Unopened Containers
 
Descriptive Properties
ColorWhite or Blue
Vertical Sag Resistance,No Sag21°C (70°F) and 375 µm (15 mil)

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PPTCHS019x / 239857

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.