Characteristics: High shock resistant ( high impact strength ) High Mechanical StrengthHigh Dielectric StrengthHigh Electrical Insulation Color- pale brown Medium flow Applications: Electric motor end shield Electrical panel components to withstand high impact High mechanical strength laminated sheetsMoulded items to withstand high mechanical shock Automotive lamp capsMoudlings exposed to warm & humid climateMoulding exposed to low intensity flame and spark, etc.Grinding disc centres CastorsGas meter partsGas regulator knobs, etc.