MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Momentive Performance Materials Silopren Electro 1700 Silicone rubber
Categories: Polymer; Thermoset; Silicone; Silicone Rubber

Material Notes: The Silopren Electro 1700 and 1800 are one-component heat curable rubber materials for making elastomers (HCE) with a hardness of 70 and 77 Shore A. These silicone rubbers are based on a platinum cure system, especially developed for the manufacture of housing and weather sheds for all kinds of insulators.

Features: One-component, ready to use. Fast vulcanization/addition curing system. Outstanding ageing behavior and weather resistance. Fast hydrophobic transfer and hydrophobic recovery. Excellent dielectric behavior over a wide range of temperatures. Very good tracking resistance. Shelf life of 3 months from date of manufacturing.

Information provided by Momentive Performance Materials.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.57 g/ccUncured; DIN 53 479 A
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore A 70DIN 53 505
Tensile Strength 5.00 MPaDIN 53 504 S2
Elongation at Break 250 %DIN 53 504 S2
Tear Strength 16.3 kg(f)/cmASTM D 624
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 1.00e+15 ohm-cm
Dielectric Constant 3.6
@Frequency 50 Hz
Cured
Dissipation Factor 0.020
 
Descriptive Properties
ColorGrayUncured. Others on request.
Tracking ResistanceClass 1A4.5IEC 60587. Vulcanization Rubber

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PMOMEN9968 / 265783

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.