MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

(Viewing data as-entered. Click here to return)
AISI Type T1 Tungsten-Alloy High-Speed-Tool Steel (UNS T12001)
Categories: Metal; Ferrous Metal; Tool Steel

Material Notes: Fe-18W-1.1V-4.13Cr-0.75C

Key Words: UNS T12001
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 8.67 g/cc
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell C 63 - 65
 30
@Temperature 649 °C
 54
@Temperature 538 °C
 60
@Temperature 427 °C
 63
@Temperature 316 °C
 64.5
@Temperature 204 °C
 65.5
@Temperature 93.3 °C
 66
@Temperature -17.8 °C
Hardness, Vickers 310
@Temperature 649 °C
 590
@Temperature 538 °C
 700
@Temperature 427 °C
 780
@Temperature 316 °C
 815
@Temperature 204 °C
 850
@Temperature 93.3 °C
 860
@Temperature -17.8 °C
 
Thermal PropertiesOriginal ValueComments
CTE, linear 9.70 µm/m-°C
Thermal Conductivity 20.0 W/m-K
 
Processing PropertiesOriginal ValueComments
Processing Temperature 540 - 595 °CTempering Temperature
 1260 - 1300 °CHardening Temperature
Annealing Temperature 870 - 900 °C
 
Component Elements PropertiesOriginal ValueComments
Carbon, C 0.75 - 0.80 %
Chromium, Cr 3.75 - 4.5 %
Iron, Fe 73.8 - 77.7 %As Balance
Manganese, Mn 0.10 - 0.40 %
Phosphorus, P <= 0.030 %
Silicon, Si 0.20 - 0.40 %
Sulfur, S <= 0.030 %
Tungsten, W 17.25 - 18.75 %
Vanadium, V 0.90 - 1.3 %
 
Descriptive Properties
Quench MediumO, A, S

References for this datasheet.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
ASTM A209 T1 Alloy Steel, Chromium Molybdenum
AISI Type M2 Molybdenum High Speed Tool Steel (UNS T11302)
AISI Type A2 Tool Steel
AISI Type M1 Molybdenum-Alloy High-Speed-Tool Steel (UNS T11301)
AISI Type M3 Class 1 Molybdenum High Speed Tool Steel (UNS T11313)

MSTT1 / 100274

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.