MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

(Viewing data as-entered. Click here to return)
Manifattura Cattaneo PET+PTFE Polyethylene Terephthalate
Categories: Polymer; Thermoplastic; Polyester, TP; Polyethylene Terephthalate (PET)

Material Notes: Manifattura Cattaneo products are available in semi-finished forms such as bars, profiles, sheets and plates.

Information provided by Manifattura Cattaneo s.p.a.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.46 g/ccISO 1183
Moisture Absorption at Equilibrium 0.23 %
@Temperature 23.0 °C
50% RH; ISO 62
Water Absorption at Saturation 0.47 %ISO 62
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell M 94ISO 2039-2
Tensile Strength at Break 76.0 MPaISO 527
Elongation at Break 7.0 %ISO 527
Tensile Modulus 3450 MPaISO 527
Compressive Yield Strength 24.0 MPa
@Strain 1 %
ISO 604
Poissons Ratio 0.44
Charpy Impact Unnotched >= 30.0 kJ/m²ISO 179
Charpy Impact, Notched 2.50 kJ/m²ISO 179
Coefficient of Friction, Dynamic 0.17on polished steel; MPC Test
Coefficient of Friction, Static 0.090on polished steel; MPC Test
K Factor (Wear Factor) 4.9 - 8.0µm/s. PV = 0.1 MPa-m/s; max P = 25 MPa; MPC Test
Limiting Pressure Velocity 0.540 MPa-m/secwithout lubrication; MPC Test
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity >= 1.00e+17 ohm-cmIEC 60093
Surface Resistance >= 1.00e+14 ohmIEC 60094
Dielectric Constant 3.2
@Frequency 1e+6 Hz
IEC 60250
Dielectric Strength 21.0 kV/mm
@Thickness 2.00 mm
IEC 60243
Dielectric Loss Index 0.014
@Frequency 1e+6 Hz
IEC 60250
 
Thermal PropertiesOriginal ValueComments
CTE, linear 85.0 µm/m-°C
@Temperature 23.0 - 100 °C
ASTM D696
Thermal Conductivity 0.290 W/m-KDOM 52612
Maximum Service Temperature, Air 115 °C
Deflection Temperature at 1.8 MPa (264 psi) 75.0 °CISO 75
Minimum Service Temperature, Air -20.0 °C
Flammability, UL94 HB
 V-2
Oxygen Index 25 %ISO 4589
 
Compliance PropertiesOriginal ValueComments
FDA Yes
 
Descriptive Properties
ColorGray Pearl
UV ResistanceN

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Celanese Rynite® 408 NC010 PET (Extended Tabular Temperature Data)
GEHR Plastics PET Polyethylene Terephthalate
Lotte Advanced Materials Infino® AE-2230 PC/PET, 20% MF
Lotte Advanced Materials Infino® ASF-9810F PBT/PET/MF
Overview of materials for Acrylic, General Purpose, Molded

PMANIF908 / 156188

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.