MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

(Viewing data as-entered. Click here to return)
Nouryon TMAl Solar Trimethylaluminum
Categories: Other Engineering Material

Material Notes: TMAL Solar is a special trimethylaluminum grade used to create an aluminum oxide passivation layer to increase efficiency of crystalline silica solar cells with proven performance in Chemical Vapour Deposition (CVD) and Atomic Layer Deposition (ALD) used in the solar cell industry.

CAS number: 75-24-1

EINECS/ELINCS No: 200-853-0

Applications: For the solar cell manufacturing industry we offer a special trimethylaluminum grade under the trade name of TMAL Solar. TMAL Solar is used to create an aluminum oxide passivation layer to increase efficiency of solar cells. TMAL Solar has proven performance in Chemical Vapour Deposition (CVD) and Atomic Layer Deposition (ALD) used in the solar cell industry. It offers a cost-effective alternative to the ultra pure trimethylaluminum used in the semiconductor industry. Not to forget its superior performance over industrial grade TMAL used in the plastics industry. The extra purification step to produce TMAL Solar guarantees consistent, high quality material for your solar cell application. Our trimethylaluminum is supplied in canisters (cylinders) made from stainless steel with an electropolished internal finish. The cylinders are equipped with manual or pneumatic diaphragm valves. The valves are equipped with metal gasket VCR connections

Information provided by Nouryon

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.743 g/cc
Viscosity 0.90 cP
Molecular Weight >= 72.1 g/mol
Vapor Pressure 0.00649 bar
@Temperature 10.0 °C
 0.00870 bar
@Temperature 15.0 °C
 
Thermal PropertiesOriginal ValueComments
Heat of Vaporization 247 J/g?Hv, NBP / 1 bar
Specific Heat Capacity 2.213 J/g-°C
@Temperature 57.0 °C
Melting Point 15.0 °C
Boiling Point 127 °C
@Pressure 0.101325 MPa
Heat of Formation -151 kJ/mol?Hf°, 25 °C / 1 bar
 
Descriptive Properties
AppearanceClear, colorless liquid
Heat of combustion-3180 kJ/moleΔHc°, 25 °C

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PNOURY950 / 286473

Ensinger PEI

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.