Description: Peel ply. Ideally suited to aerospace phenolic resin applications. Features & Benefits: - Porous, medium weight polyester peel ply
- Heat set and scoured, for use directly against laminates or bond lines
- Available coated or non-coated depending on user requirement
- Recommended for composite manufacture and metal bonding applications
- Colored dark green for ease of detection on cured laminate
- Recommended for use with phenolic resins
- Imparts a coarse weave pattern upon removal from the laminate
Information provided by Cytec, subsequently acquired by Solvay. |