MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
BASF Styroblend® WS 2776 Impact Grade Polystyrene Blend  (discontinued **)
Categories: Polymer; Thermoplastic; Polystyrene (PS); Polystyrene, Impact Modified

Material Notes: PS/PE blend with high stress-cracking resistance and low permeability to water vapor. Used for making tough packaging components, suitable for coextrusion with PE, PS, e.g. for milk portions.

Data was collected by ISO methods and provided by BASF.

Styroblend® is no longer part of the BASF product line.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.990 g/cc
Water Absorption 0.10 %
Moisture Absorption at Equilibrium 0.10 %
Linear Mold Shrinkage, Flow 0.0065 cm/cm
Melt Flow 4.0 g/10 min
@Load 5.00 kg,
Temperature 200 °C
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength, Yield 27.0 MPa
Elongation at Break >= 50 %
Elongation at Yield 4.0 %
Tensile Modulus 1.20 GPa
Charpy Impact Unnotched NB
 NB
@Temperature -30.0 °C
Charpy Impact, Notched 2.00 J/cm²
 
Electrical PropertiesOriginal ValueComments
Electrical Resistivity 1.00e+14 ohm-cm
Surface Resistance 1.00e+13 ohm
Dielectric Constant 2.5
@Frequency 100 Hz
 2.5
@Frequency 1e+6 Hz
 
Thermal PropertiesOriginal ValueComments
Vicat Softening Point 79.0 °C
Flammability, UL94 HB
@Thickness 3.20 mm

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PSF233 / 66814

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.