MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Buckeye Polymers BP RPPC 1813 C BLK Polypropylene, Calcium Filled
Categories: Polymer; Thermoplastic; Polypropylene (PP); Polypropylene with 10% Calcium Carbonate (CaCO3) Filler

Material Notes: Product Information: Calcium Carbonate Filled PP Grades have a high impact toughness, moderate increased stiffness, and excel in high gloss applications. Our BP RPP C series product line ranges from 10-50% in filler levels. These materials can be customized through the addition of UV packages, custom matching, and processing additives.

    Product Features:
  • Can be UV stabilized for increased resistance
  • Industrial, outdoor furniture, and window trim.
  • Forms: Square Stand Cut Pellets, Round Gala Cut Pelllets

    Processing Method: Injection Moulding

    Information Provided by Buckeye Polymers, Inc.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Linear Mold Shrinkage 0.011 - 0.0135 in/inASTM D955
Melt Flow 10 - 16 g/10 minASTM D1238
Ash 16 - 20 %ASTM D5630
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength, Yield >= 2000 psiASTM D638
Flexural Modulus >= 140000 psiASTM D790
Izod Impact, Notched >= 0.900 ft-lb/inASTM D256
Gardner Impact >= 50.0 ft-lbASTM D5420

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Buckeye Polymers BP RPPC 1020 TU BLK Polypropylene Copolymer
Ravago Manufacturing Americas Echo® RPPC 20/2 BK Recycled Polypropylene
Buckeye Polymers BP RPPC 2010 CW Polypropylene, Calcium Filled
Polyram RamOfin RPPC711 Polypropylene, UV Stabilized
Ravago Manufacturing Americas Echo® RPPC 30/2 BK Recycled Polypropylene

PBUCK004 / 104472

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.