Master Bond UV15X-6Med-2LV is a one component, medium viscosity UV system featuring high flexibility, excellent toughness and superior abrasion resistance. It can be used for a wide variety of applications including bonding, sealing, coating and encapsulation. Its robust flexibility allows it to withstand severe thermal cycling as well as resisting thermal and mechanical shocks. UV15X-6Med- 2LV bonds well to a variety of substrates, especially glass, polycarbonates and acrylics as well as many other plastics, metals and rubbers. It has good chemical resistance to water, cleaning agents, chemical sterilants, EtO and gamma radiation. UV15X-6Med-2LV is a top notch thermal and electrical insulator with a service temperature range of -80°F to +250°F. UV15X-6Med-2LV generally cures readily in 10-30 seconds when exposed to a UV light source emitting at a wavelength of 320-365 nm with an energy output as low as 20-40 milliwatts/cm². The rate of cure depends upon the system’s distance from the light source, the thickness of the section and of course the intensity of the light source. It should be noted that the system can cure in sections approaching 1/4 inch thick. However, when bonding, sections of a few thousandths of an inch are more than adequate. Most importantly, UV15X-6Med-2LV does not display oxygen inhibition. This system is widely used in medical device manufacturing and specialty applications where ISO 10993-5 requirements are desirable. Product Advantages: - One part system with no mixing needed
- Cures fast upon exposure to 320-365 nm UV light at ambient temperatures. No oxygen inhibition
- Outstanding toughness and abrasion resistance
- Withstands rigorous thermal cycling
- Passes ISO 10993-5 for cytotoxicity
Key Features: - Superior abrasion resistance
- Meets ISO 10993-5
- High flexibility and toughness
- Moderate viscosity
Information provided by Master Bond. |
Master Bond is a leading manufacturer of adhesives, sealants, coatings and potting compounds. Master Bond’s vast product line consists of over 3,000 epoxy, polyurethane, silicone, cyanoacrylate and latex adhesives that vary in viscosity, cure speed, strength, chemical resistance, electrical properties, etc. Our custom adhesives offer design flexibility and provide excellent bonding performance. Visit www.masterbond.com.Click here to view all available suppliers for this material. Please click here if you are a supplier and would like information on how to add your listing to this material. |