MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

(Viewing data as-entered. Click here to return)
Celanese Celstran® PA66-GF40-02 40% Long Glass Fiber Reinforced Nylon 6/6
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 66 (PA66); Nylon 66, 40% Glass Fiber Filled

Material Notes: Description: 40% long strand glass fiber reinforced heat stabilized Nylon 6/6

Information provided by Celanese Corporation.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.45 g/ccISO 1183 & ASTM D792
Linear Mold Shrinkage 0.0010 - 0.0020 cm/cmASTM D955
Linear Mold Shrinkage, Transverse 0.0020 - 0.0030 cm/cmASTM D955
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break 215 MPa5 mm/min; ISO 527-2/1A
 36700 psiASTM D638
 39100 psi
@Temperature -40.0 °C
ASTM D638
Tensile Strength, Ultimate 19400 psi
@Temperature 121 °C
ASTM D638
Elongation at Break 2.0 %5 mm/min; ISO 527-2/1A
 2.3 %ASTM D638
 2.2 %
@Temperature -40.0 °C
ASTM D638
 2.5 %
@Temperature 121 °C
ASTM D638
Tensile Modulus 13.3 GPa1 mm/min; ISO 527-2/1A
 2.06e+6 psiASTM D638
 1.06e+6 psi
@Temperature 121 °C
ASTM D638
 2.10e+6 psi
@Temperature -40.0 °C
ASTM D638
Flexural Strength 355 MPaISO 178
 52000 psiASTM D790
 26300 psi
@Temperature 121 °C
ASTM D790
 56300 psi
@Temperature -40.0 °C
ASTM D790
Flexural Modulus 11.8 GPaISO 178
 1.78e+6 psiASTM D790
 940000 psi
@Temperature 121 °C
ASTM D790
 1.805e+6 psi
@Temperature -40.0 °C
ASTM D790
Izod Impact, Notched 6.90 ft-lb/inASTM D256
 8.70 ft-lb/inat 250°F; ASTM D256
 7.40 ft-lb/in
@Temperature -40.0 °C
ASTM D256
Charpy Impact, Notched 3.50 J/cm²ISO 179/1eA
 
Thermal PropertiesOriginal ValueComments
Deflection Temperature at 1.8 MPa (264 psi) 255 °CISO 75-1, -2 & ASTM D648

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Akro-Plastic Akromid® B3 GF 40 (2474) PA 6 Dry, 40% Glass Filled
Domo Technyl® A 216 V40 40% Glass Filled Nylon 66
MTI ThermoStran® PA66-30C Long Carbon Fiber Compound
BASF Capron® GR40 40% Glass-Filled Nylon 6 (Conditioned)
Overview of materials for Nylon 66, 40% Glass Fiber Filled

PHCV17 / 45857

Ensinger PEI

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.