MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Wingate Alloys Winco HCC High Carbon, High Chrome Tool and Die Steel
Categories: Metal; Ferrous Metal; Carbon Steel; High Carbon Steel; Tool Steel; Cold Work Steel

Material Notes: A cold working, high output tool steel highly resistant to wear.
    Advantages:
  • Due to high carbon and chrome content is a must on high production runs.
  • Deep hardening steel with the absolute minimum of distortion.
  • Excellent machinability and high compressive strength.
  • Can be tempered to approximate hardness of 61-63 Rc.
Applications: Blanking dies, extrusion dies, stamping dies, coining dies, knurling dies, swaging dies, crimping dies, lamination dies, threading dies, drawing dies, slitting dies, trimming dies, broaches, hobs, punches, bushing, reamers, forming rolls, seaming rolls, gauges and taps.

Information from Wingate Alloys Inc.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell C 61 - 63Tempered

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
AISI Type D7 Air-Hardening Cold-Work Tool Steel (UNS T30407)
Overview of materials for Maraging Steel
AISI Type A3 Tool Steel
International Mold Steel Premium H13 Hot Work Die and Mold Steel
AISI Type A6 Tool Steel, austenitized 830-870°C (1525-1600°F)

NWINGA29 / 122093

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.