MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

(Viewing data as-entered. Click here to return)
MAS Epoxies TABLE TOP PRO Two-component epoxy system 100% solids
Categories: Polymer; Thermoset; Epoxy

Material Notes: The MAS Table Top Pro Epoxy System is a 100% solids, two-component system. It has a one-to-one by volume mix ratio and cures at room temperature. It can be used for tabletops, bar tops and art. It cures to a clear, glass-like finish that resists scratching and yellowing. The system demonstrates excellent anti-blushing properties and will not distort with age. Cures clear for a high-gloss durable finish, Ideal for bars and tabletops to protect wood from damage, Versatile product can be used on art, tables, small castings and other projects.

Information provided by MAS Epoxies.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.11 g/ccCured; ASTM D792
 8.10 lb/galHardener; ASTM D1475
Viscosity 1750 cPHardener; ASTM D2196
 3500 cPInitial Mixed; ASTM D2196
 9000 cPResin; ASTM D2196
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore D 82ASTM D2240
Tensile Strength 7400 psiASTM D638
Elongation at Break 5.9 %ASTM D638
Tensile Modulus 382000 psiASTM D638
Flexural Strength 12800 psiASTM D790
Flexural Modulus 373000 psiASTM D790
Compressive Strength 10400 psiASTM D695
Izod Impact, Notched 0.760 ft-lb/inASTM D256
 
Thermal PropertiesOriginal ValueComments
Maximum Service Temperature, Air 118 °FHDT load unknown, room temp cure; ASTM D648
 124 °FHDT load unknown, post cure; ASTM D648
Shrinkage 3.85 %ASTM D792/2196 (volumetric)
 
Processing PropertiesOriginal ValueComments
Gel Time 30.0 min150g mass; ASTM D2471
 
Descriptive Properties
ColorClear
Mix Ratio by Volume1A : 1B
Mix Ratio by Weight100A : 83B
Volumetric Yield (in³/lb)25ASTM D792

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PMASZ901 / 265516

Ensinger PEI

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.