MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Extreme Materials from MCAM
Visit Mitsubishi Chemical Advanced Materials for Extreme Materials - high performance plastic machining stock engineered to replace metals such as nickel alloys or stainless steel.

(Viewing data as-entered. Click here to return)
Bales Mold Service Ni-Hard® (Nickel-Cobalt) Mold Coating
Categories: Metal; Nonferrous Metal; Nickel Alloy; Other Engineering Material; Ceramic/Metallic Coating

Material Notes: Description: NiHard® is made up of an ultra pure chemistry of Nickel and Cobalt that offers extreme wear resistance and longer mold life.

Applications: Uniform deposit for complex details and good chrome alternative.

Information provided by Bales Mold Service Inc.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell C 62
Coefficient of Friction <= 0.24
 
Processing PropertiesOriginal ValueComments
Processing Temperature 185 °FApplied Temperature

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
MetalTek IN® 909 Centri-Vac Nickel Cobalt Based Alloy
AISI 8640 Steel, oil quenched 845°C (1550°F), 540°C (1000°F) temper, 100 mm (4 in.) round
AISI 8630 Steel, quenched 855°C (1570°F), 425°C (800°F) temper
AISI 8630 Steel, oil quenched 845°C (1550°F), 455°C (850°F) temper
AISI 5140 Steel, oil quenched 845°C (1550°F), 595°C (1100°F) temper, 100 mm (4 in.) round

NBAL2 / 15081

New MatWeb Services

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.