MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

(Viewing data as-entered. Click here to return)
Nouryon Armogel T
Categories: Other Engineering Material

Material Notes: Surfactant-based acid gelling agent stable to temperatures of 300F/149C for oilfield stimulation applications.

Information provided by Nouryon

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.890 g/cc
Viscosity 75 cP
@Temperature 35.0 °C
Surface Tension 28 dynes/cmaccording to Du Noüy, 25°C, 0.1%; DIN 53914
 
Thermal PropertiesOriginal ValueComments
Melting Point 30.0 - 40.0 °C
Pour Point 30.0 °C
Flash Point >= 100 °C
 
Optical PropertiesOriginal ValueComments
Gardner Color Number <= 6.0
 
Component Elements PropertiesOriginal ValueComments
H2O, Water <= 1.0 %
 
Descriptive Properties
AppearanceLiquid/paste
Clear point32 °C
Content= 97 %Tertiary Amine
Content(%)100Active content
Equivalent mass340-360
Foam Height according to Ross-Miles2 mmafter 5 min, 50°C, 0.05%
 5 mmimmediately, 50°C, 0.05%
Wetting power=600 secaccording to Draves, 25°C, 0.1%

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PNOURY243 / 285766

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.