Eraclene MM 74 is a high density polyethylene resin (HDPE) with antioxidants, suitable for injection molding application. Eraclene MM 74 is characterized by a good balance between rigidity and impact resistance. The resin is UV stabilized and is recommended for the production of items for outdoor exposure. Main Applications: Eraclene MM 74 is specifically designed for pails, lids for light-weight containers, agricultural containers, houseware and dust bins. Information provided by Polimeri Europa. Versalis is the Eni subsidiary containing the plastics and rubber businesses. |