MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
3M 32661 Heavy Duty Performance Coating - Part B
Categories: Polymer; Thermoset; Rubber or Thermoset Elastomer (TSE)

Material Notes: 3M™ HD (Heavy Duty) Performance Coating is 100% solids elastomeric lining especially developed for high abrasion and tear resistance with thick build up characteristics. It has good durability and adhesion to metal, fiberglass, aluminum, wood (plywood, OSB, etc.), concrete and masonry. It is a two component 1:1 by volume system with adhesion enhancement chemical complexes. The protective coating can be applied up to 500 mil thick and offers an ultra-fast cure that speeds production in an OEM setting. This aromatic formulation displays excellent chemical and environmental resistance while reducing the moisture problem that causes bubbling. It also offers high elongation and flexibility the produces high impact resistance. Neutral Part B is a lightly yellowish/translucent color and is design to be tinted by the customer (at the customer’s own risk) to the color required. Follow the manufacture of the tinting bases recommendation for percent loading of the color tint.

Information provided by 3M

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.01 - 1.05 g/cc
Solids Content 100 %
Water Absorption <= 1.78 %ASTM D570
Brookfield Viscosity 150 - 1250 cPRVT Model, Spindle #3 @ 20 rpm
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore D 54 - 60ASTM D2240
Tensile Strength at Break 12.4 - 15.2 MPaASTM 638-01
Elongation at Break 93 %ASTM 638-01
Tear Strength 50.9 - 59.8 kg(f)/cmASTM D624
Taber Abrasion, mg/1000 Cycles 35 - 40ASTM D40695
Tangent Modulus 16000 - 18000 psiTangent; ASTM 638-01
 
Thermal PropertiesOriginal ValueComments
Maximum Service Temperature, Air 93.0 °C
Minimum Service Temperature, Air -29.0 °C
Flash Point 93.0 °C
 
Processing PropertiesOriginal ValueComments
Cure Time 60.0 - 120 minlight use
 1440 minheavy duty use
Shelf Life 12.0 Month
@Temperature 21.0 - 32.0 °C

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Overview of materials for Thermoset Fluoroelastomer
CHT Group EP RAP-1567 SP EPI Engineered Polymers Silicone Aliphatic Polyurea
3M 32660 Heavy Duty Performance Coating - Part A

PMM34310 / 169057

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.