MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

(Viewing data as-entered. Click here to return)
Petropol Tenogel® A3 HF PRTA010 AB324 ABS
Categories: Polymer; Thermoplastic; ABS Polymer; Acrylonitrile Butadiene Styrene (ABS), Molded

Material Notes: Product Description: High Flow, ABS

Resin ID (ISO 1043): ABS
Additive: High Flow
Processing: Injection Molding
Color: Black

Information provided by Petropol

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.05 g/ccASTM D792
Water Absorption 0.30 %ASTM D570
Linear Mold Shrinkage 0.0040 - 0.0060 cm/cm
@Thickness 3.20 mm
ASTM D955
Melt Flow 20 - 30 g/10 min
@Load 10.0 kg,
Temperature 220 °C
ASTM D1238
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell R 116ASTM D785
Tensile Strength, Yield 49.0 MPa5mm/min; ASTM D638
Elongation at Break 35 %5mm/min; ASTM D638
Flexural Strength 76.0 MPa3mm/min; ASTM D790
Flexural Modulus 2450 MPa3mm/min; ASTM D790
Izod Impact, Notched 196 J/mASTM D256
 
Thermal PropertiesOriginal ValueComments
CTE, linear 71.0 µm/m-°CASTM D696
Thermal Conductivity 0.150 W/m-KASTM C177
Deflection Temperature at 1.8 MPa (264 psi) 92.0 °CASTM D648
Vicat Softening Point 100 °CASTM D1525
Flammability, UL94 HB
 
Processing PropertiesOriginal ValueComments
Processing Temperature 190 - 230 °CInjection
Mold Temperature 50.0 - 70.0 °C
Drying Temperature 85.0 °C
Dry Time 3.00 hour

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PPETROPOL347 / 313255

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.