Westlake EF 563 resin is a fractional melt index 6.5% EVA copolymer with excellent drawdown, low melting/dispersion, and clarity optics in a soft but very tough film. Kosher compliant.Application/Uses- Film packaging
- Batch inclusion bags
FDA: This material complies with FDA regulations in 21 CFR, section 177.1350.All information provided by Westlake Chemical |
Excellent drawdown, low melting/dispersion, and clarity optics. 6.5% EVA. |