MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

(Viewing data as-entered. Click here to return)
SABIC NORYL™ Resin NHP9023 Polyphenylene Ether + PS (PPE+PS) (Europe)
Categories: Polymer; Thermoplastic; Polystyrene (PS); Polystyrene + Polyphenylene Ether, Unreinforced

Material Notes: NORYL™ NHP9023 resin is a 15% glass reinforced blend of polyphenylene ether (PPE) + high impact polystyrene (HIPS). This injection moldable grade contains non-brominated, non-chlorinated flame retardant and carries a UL94 flame rating of V0 1.5mm and V1 at 0.75mm for thin-wall molding capability. NORYL NHP9023 is based on a unique co-polymer technology and exhibits good dimensional stability, high heat resistance, strong electrical performance, and very low specific gravity. It is an excellent candidate for copier fuser units, business equipment internal components, and electrical applications where thin-wall FR, modulus retention, and high heat resistance are required.

Features: Hydrolytic Stability,Low Creep Sensitivity,High Heat Resistance,Good Stiffness,Non-Halogenated,Non-Chlorinated,Non-Brominated,Low Warpage,Good Processability,Structural

Information provided by SABIC

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.21 g/ccASTM D792
Density 1.21 g/ccISO 1183
Moisture Absorption 0.0200 %Injection Molding
 0.110 %23°C / 50% RH; ISO 62
Water Absorption at Saturation 0.20 %ISO 62-1
Viscosity 17 cP
@Load 10.0 kg,
Temperature 280 °C
MVR cc/10 min; ISO 1133
Linear Mold Shrinkage, Flow 0.0038 cm/cmSABIC method
Melt Flow 20 g/10 min
@Load 5.00 kg,
Temperature 300 °C
ASTM D1238
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell R 121ASTM D785
Tensile Strength at Break 90.0 MPa5 mm/min; ISO 527
 112 MPa5 mm/min; ASTM D638
Elongation at Break 2.7 %5 mm/min; ISO 527
 2.9 %5 mm/min; ASTM D638
Tensile Modulus 5400 MPa5 mm/min; ASTM D638
 5500 MPa1 mm/min; ISO 527
Flexural Strength 140 MPayield, 2 mm/min; ISO 178
 163 MPayld, 1.3 mm/min, 50 mm span; ASTM D790
Flexural Modulus 4900 MPa2 mm/min; ISO 178
 5200 MPa1.3 mm/min, 50 mm span; ASTM D790
Izod Impact Notched 500 JASTM D256
Izod Impact, Notched (ISO) 7.00 kJ/m²80*10*4; ISO 180/1A
 6.00 kJ/m²
@Temperature -30.0 °C
80*10*4; ISO 180/1A
Izod Impact, Unnotched (ISO) 27.0 kJ/m²80*10*4; ISO 180/1U
 28.0 kJ/m²
@Temperature -30.0 °C
80*10*4; ISO 180/1U
Charpy Impact Unnotched 27.0 kJ/m²Edgew 80*10*3 sp=62mm; ISO 179/1eU
 31.0 kJ/m²
@Temperature -30.0 °C
Edgew 80*10*3 sp=62mm; ISO 179/1eU
Charpy Impact, Notched 7.00 kJ/m²Edgew 80*10*4 sp=62mm; ISO 179/1eA
 
Electrical PropertiesOriginal ValueComments
Comparative Tracking Index 175 VIEC 60112
 
Thermal PropertiesOriginal ValueComments
CTE, linear, Parallel to Flow 35.0 µm/m-°C
@Temperature 23.0 - 80.0 °C
ISO 11359-2
 38.0 µm/m-°C
@Temperature -40.0 - 40.0 °C
ISO 11359-2
CTE, linear, Transverse to Flow 64.0 µm/m-°C
@Temperature 23.0 - 80.0 °C
ISO 11359-2
Hot Ball Pressure Test 125 °CPASS; IEC 60695-10-2
Deflection Temperature at 1.8 MPa (264 psi) 153 °C
@Thickness 6.40 mm
unannealed; ASTM D648
Vicat Softening Point 161 °CRate B/50; ISO 306
 163 °CRate B/120; ISO 306
Glow Wire Flammability Index 960 °C
@Thickness 3.20 mm
IEC 60695-2-12
 
Processing PropertiesOriginal ValueComments
Nozzle Temperature 300 - 325 °C
Zone 2 275 - 320 °C
Zone 3 290 - 325 °C
Melt Temperature 300 - 325 °CInjection Molding
Mold Temperature 80.0 - 110 °C
Drying Temperature 110 - 120 °CInjection Molding
Dry Time 3.00 - 4.00 hourInjection Molding
 8.00 hourCumulative; Injection Molding
Back Pressure 0.300 - 0.700 MPa
Shot Size 30 - 70 %
Screw Speed 20 - 100 rpm

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PSABH82409 / 290356

Ensinger PEI

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.