MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
ExxonMobil Santoprene® 211-45 Thermoplastic Elastomer
Categories: Polymer; Thermoplastic; Elastomer, TPE; Thermoplastic Vulcanizate Elastomer (TPV)

Material Notes: A soft, colorable, versatile thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. This material combines good physical properties and chemical resistance for use in a wide range of injection molding applications. This grade of Santoprene TPV is shear-dependent and can be processed on conventional thermoplastics equipment for injection molding. It is polyolefin based and completely recyclable.

Key Features:

  • Recommended for applications requiring excellent flex fatigue resistance.
  • Excellent ozone resistance.
  • UL listed: file #QMFZ2.E80017, Plastics - Component; file #QMFZ8.E80017, Plastics Certified For Canada - Component.
  • Although not NSF certified, this product has a Material Supplier Form on file with NSF to facilitate its evaluation for use in applications requiring NSF certification.
  • Used in sealing applications.
  • EU and China RoHS compliant.
Applications:
  • Automotive – Grips, Interior Mat, Seals and Gaskets
  • Soft Touch Grips
  • Tubing
Uses:
  • Automotive Applications
  • Gaskets
  • Seals
Availability: Africa & Middle East, Europe, North America, Asia Pacific, Latin America and South America

Information provided by ExxonMobil Chemical

Key Words: EU 2003/11/EC; RoHS Compliant; UL QMFZ2; UL QMFZ8
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 0.960 g/ccASTM D792
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore A 492 mm, 15 sec; ISO 868
 50Air at 302°F, 168 hr; ASTM D573
Tensile Strength at Break 391.2 psiAir at 302°F, 168 hr; ASTM D573
 508 psiAcross Flow; ASTM D412
Tensile Stress at Strain 203 psi
@Strain 100 %
Across Flow; ISO 868
Elongation at Break 340 %Across Flow; ASTM D412
 428.4 %Air at 302°F, 168 hr; ASTM D573
Compression Set 11 %
@Temperature 22.8 °C,
Time 79200 sec
ASTM D395
 35 %
@Temperature 125 °C,
Time 252000 sec
ASTM D395
 
Electrical PropertiesOriginal ValueComments
Dielectric Constant 2.42.03 mm; ASTM D150
Dielectric Strength 770 V/mil2.03 mm; ASTM D149
 
Thermal PropertiesOriginal ValueComments
Brittleness Temperature -80.0 °FASTM D746
UL RTI, Electrical 100 °CUL 746
UL RTI, Mechanical with Impact 90.0 °C
@Thickness 1.00 mm
UL 746
 95.0 °C
@Thickness 3.00 mm
UL 746
Flammability, UL94 HB
@Thickness 1.00 mm
 HB
@Thickness 3.00 mm
 
Processing PropertiesOriginal ValueComments
Processing Temperature 175 - 230 °C
Rear Barrel Temperature 350 - 380 °F
Middle Barrel Temperature 355 - 390 °F
Front Barrel Temperature 355 - 400 °F
Nozzle Temperature 375 - 445 °F
Melt Temperature 380 - 465 °FProcessing
Mold Temperature 50.0 - 125 °FProcessing
Drying Temperature 180 °F
Dry Time 3 hour
Moisture Content 0.080 %
Back Pressure 50.0 - 100 psiProcessing
Clamp Pressure 6000 - 10000 psi
Vent Depth 0.00100 in
Cushion 0.125 - 0.250 in
Screw Speed 100 - 200 rpm
 
Descriptive Properties
ColorNatural Color
FormPellets
Injection RateFast
Maximum Regrind %20
Screw Compression Ratio2:1 - 2.5:1
Screw L/D Ratio16:1 - 20:1

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
AISI 1045 Steel, turned, ground, and polished, 19-32 mm (0.75-1.25 in) round
ExxonMobil Santoprene® 111-45 Thermoplastic Elastomer
ExxonMobil Santoprene® 8211-35 Thermoplastic Elastomer
Overview of materials for Acrylonitrile Butadiene Styrene (ABS), Molded
RheTech Products G10P100-00 10% Glass Fiber Reinforced Polypropylene, Natural

PADVA100 / 22790

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.