MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Teknor Apex Beetle® PET166F Polyethylene Terephthalate, 30% Glass Fiber Reinforced
Categories: Polymer; Thermoplastic; Polyester, TP; Polyethylene Terephthalate (PET); Polyethylene Terephthalate (PET), 30% Glass Reinforced

Material Notes: Notes: PET166F is a 30% glass fiber reinforced grade of PET that offers good mechanical performance at elevated temperature and excellent mold release.

Processing Method: Injection Molding

Forms: Pellets

Injection Notes: Drying is necessary if material has been exposed to air for longer than 3 hours; Back Pressure: Low; Injection Pressure; High; Injection Rate: Fast

Information Provided by Teknor Apex

Key Words: PET
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Thermal PropertiesOriginal ValueComments
Flammability, UL94 HB
@Thickness 1.57 mm
 
Processing PropertiesOriginal ValueComments
Rear Barrel Temperature 500 - 536 °F
Middle Barrel Temperature 500 - 536 °F
Front Barrel Temperature 500 - 536 °F
Melt Temperature <= 554 °FProcessing Temperature
Mold Temperature 248 - 284 °F
Drying Temperature 284 °F
Dry Time 4 hour
Screw Speed 50 - 100 rpm

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Shinkong Synthetic Fibers Shinite® T101G30 PET, 30% Glass Filled
Samyang Tripet® 2500G30 Polyethylene Terephthalate, 30% Glass Fiber Reinforced
RTP Company RTP 1105 FR Polyethylene Terephthalate (PET), Glass Fiber - Flame Retardant - UL94 V-0
RTP Company RTP 1105  Polyethylene Terephthalate (PET) Glass Fiber 30%
RTP Company RTP 1100  Polyethylene Terephthalate (PET) Base Resin

PTEKNO444 / 128621

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.