MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

(Viewing data as-entered. Click here to return)
Manifattura Cattaneo PA 6.6 30% GF Nylon, Glass Filled
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 66 (PA66); Nylon 66, 30% Glass Fiber Filled

Material Notes: Manifattura Cattaneo products are available in semi-finished forms such as bars, profiles, sheets and plates.

Information provided by Manifattura Cattaneo s.p.a.

Key Words: Polyamide
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.29 g/ccISO 1183
Moisture Absorption at Equilibrium 1.7 %
@Temperature 23.0 °C
50% RH; ISO 62
Water Absorption at Saturation 5.5 %ISO 62
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell M 76ISO 2039-2
Tensile Strength at Break 75.0 MPaConditioned 50% RH; ISO 527
 100 MPaDried; ISO 527
Tensile Strength, Yield 45.0 MPaConditioned 50% RH; ISO 527
 90.0 MPaDried; ISO 527
Elongation at Break 5.0 %Dried; ISO 527
 12 %Conditioned 50% RH; ISO 527
Tensile Modulus 3200 MPaConditioned 50% RH; ISO 527
 5900 MPaDried; ISO 527
Compressive Yield Strength 28.0 MPa
@Strain 1 %
ISO 604
Charpy Impact Unnotched 50.0 kJ/m²ISO 179
Charpy Impact, Notched 6.00 kJ/m²ISO 179
Coefficient of Friction, Dynamic 0.24on polished steel; MPC Test
Coefficient of Friction, Static 0.23on polished steel; MPC Test
K Factor (Wear Factor) 3.8µm/s. PV = 0.1 MPa-m/s; max P = 28 MPa; MPC Test
Limiting Pressure Velocity 0.330 MPa-m/secwithout lubrication; MPC Test
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity >= 1.00e+15 ohm-cmIEC 60093
Surface Resistance >= 1.00e+12 ohmIEC 60094
Dielectric Constant 3.9
@Frequency 1e+6 Hz
IEC 60250
Dielectric Strength 28.0 kV/mm
@Thickness 2.00 mm
IEC 60243
Dielectric Loss Index 0.040
@Frequency 1e+6 Hz
IEC 60250
 
Thermal PropertiesOriginal ValueComments
CTE, linear 60.0 µm/m-°C
@Temperature 23.0 - 100 °C
ASTM D696
Thermal Conductivity 0.300 W/m-KDOM 52612
Maximum Service Temperature, Air 120 °C
Deflection Temperature at 1.8 MPa (264 psi) 150 °CISO 75
Minimum Service Temperature, Air -20.0 °C
Flammability, UL94 V-2
 
Compliance PropertiesOriginal ValueComments
FDA No
 
Descriptive Properties
ColorIvory
UV ResistanceNDried
 YConditioned 50% RH

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Teknor Apex Sarlink® 3160 Thermoplastic Elastomer
GEHR Plastics PA 6.6-30GF Nylon 6.6, 30% Glass Fiber, Dry
Aluminum 6061-T6; 6061-T651
Avient LubriOne™ NN-30GF/13T-2S Black Polyamide 66 (Nylon 66)
Overview of materials for Nylon 66, 30% Glass Fiber Filled

PMANIF904 / 156184

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.