MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

(Viewing data as-entered. Click here to return)
Solvay Chemicals A50 Methylene chloride
Categories: Fluid; Solvent

Material Notes: Thanks to its specific characteristics, especially high solvent power, it is used where a high-grade economic solvent is required, because it successfully dissolves many organic compounds. Its high volatility is especially recommended to extract materials sensitive towards temperature

EINECS Number: 200-838-9/CAS Number: 75-09-2/UN number: 1593

Information provided by Solvay

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.318 - 1.329 g/ccD20/4
 1.32 - 1.332 g/ccD20/20
 1.288 g/cc
@Temperature 40.0 °C
 1.297 g/cc
@Temperature 35.0 °C
 1.306 g/cc
@Temperature 30.0 °C
 1.316 g/cc
@Temperature 25.0 °C
 1.325 g/cc
@Temperature 20.0 °C
 1.334 g/cc
@Temperature 15.0 °C
 1.343 g/cc
@Temperature 10.0 °C
 1.352 g/cc
@Temperature 5.00 °C
 1.361 g/cc
@Temperature 0.000 °C
Viscosity 0.30 cP
@Temperature 30.0 °C
Dynamic
 0.36 cP
@Temperature 40.0 °C
Dynamic
 0.38 cP
@Temperature 35.0 °C
Dynamic
 0.41 cP
@Temperature 25.0 °C
Dynamic
 0.43 cP
@Temperature 20.0 °C
Dynamic
 0.46 cP
@Temperature 15.0 °C
Dynamic
 0.48 cP
@Temperature 10.0 °C
Dynamic
 0.51 cP
@Temperature 5.00 °C
Dynamic
 0.53 cP
@Temperature 0.000 °C
Dynamic
Molecular Weight 84.9 g/mol
Vapor Pressure 0.189 bar
@Temperature 0.000 °C
 0.241 bar
@Temperature 5.00 °C
 0.304 bar
@Temperature 10.0 °C
 0.379 bar
@Temperature 15.0 °C
 0.469 bar
@Temperature 20.0 °C
 0.575 bar
@Temperature 25.0 °C
 0.700 bar
@Temperature 30.0 °C
 0.847 bar
@Temperature 35.0 °C
 1.016 bar
@Temperature 40.0 °C
 
Descriptive Properties
AppearanceClear without suspended matterASMT D3741/B
Color<10APHA
Composition<1 mg/kgOxidizing Compounds (Cl2)
 <100 mg/kg1,2-Dichloroethane
 <100 mg/kg1,1-Dichloroethylene
 <12 mg/kgCarbon Tetrachloride
 <5 mg/kgAcidity (HCl)
 <50 mg/kgMoisture (H2O), Karl Fischer, ASTM E1064
 <56 mg/kgChloroform
 40-60 mg/kgStabilizer (Amylene)
Purity>999.5 g/kgwithout stabilizers

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Celanese Nilit FRIANYL A63 V0 Nylon 6.6 for injection molding
Chosun Refractories A50 Special High-Density Gunning Castable
ASTM A36 Steel, plate

WSOLV142 / 147791

Ensinger PEI

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.