MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Schott D 263® T eco Ultra-Thin Glass
Categories: Ceramic; Glass; Optical

Material Notes: SCHOTT ultra-thin glass is available in different glass types with different chemical and physical properties. It is produced with the untouched surface of Schott's continuous down-draw process.

Applications

  • Semiconductor IC Packaging and 2.5D Interposer
  • Electronic and Optical Sensors
  • Energy Storage Devices
  • Organic Electronics incl. Oxygen and Moisture Barrier
  • High Strength, Scratch Resistant Touch & Cover Glass

Information provided by SCHOTT.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 2.51 g/cc
Thickness 25.0 - 200 microns
 
Mechanical PropertiesOriginal ValueComments
Hardness, Knoop 5900.1/20
Modulus of Elasticity 72.9 GPa
 
Electrical PropertiesOriginal ValueComments
Dielectric Constant 6.3
@Frequency 5.00e+9 Hz
 6.4
@Frequency 1e+9 Hz
 6.7
@Frequency 1e+6 Hz
Dissipation Factor 0.0060
@Frequency 1e+6 Hz
 0.0070
@Frequency 1e+9 Hz
 0.010
@Frequency 5.00e+9 Hz
 
Thermal PropertiesOriginal ValueComments
CTE, linear 7.20 µm/m-°C
@Temperature 20.0 - 300 °C
Thermal Conductivity 1.06 W/m-K
@Temperature 90.0 °C
Transformation Temperature, Tg 557 °C
 
Optical PropertiesOriginal ValueComments
UV Transmittance 91 %
@Wavelength 400 nm

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Schott D 263 Thin Borosilicate Glass
Vibrantz Technologies CF 7586 Low-Temperature Sealing
Vibrantz Technologies F 2719 Metal Sealing
Schott B270™ Sheet Glass
Schott D 263® T eco Thin Borosilicate Optical Glass

CSGT9945 / 183198

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.