MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Danquinsa DANCOLOR® MB-9005/355/PU Color master batch
Categories: Other Engineering Material; Additive/Filler for Polymer

Material Notes: DANCOLOR® MB-9005/355/PU is a combined masterbatch based on TPU, which is delivered in form of even black pigmented granules (pellets). This TPU concentrate is used for pigmenting of thermoplastic polyurethanes as well as for the reaching of matt surfaces. It contains therefore already an matted additive. DANCOLOR® MB-9005/355/PU can be added to our polyurethanes based on polyester as well to our polyurethanes based on polyether. DANCOLOR® MB-9005/355/PU is suitable for the processing by extrusion, injection moulding and for melt-calendering.

Application: DANCOLOR® MB-9005/355/PU can be applied and mixed with all products out of our PEARLTHANE®- or PEARLCOAT®- range ( based on polyester or polyether ) which find their application by extrusion, injection moulding or calendering. An addition of 1 to 3% ( calculated by the weight of the TPU ) is recommended. If there is a requirement by the end product, higher doses can also be considered.

Information provided by Danquinsa GMBH

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.700 g/ccASTM D1875
Storage Temperature 15.0 - 25.0 °C
 
Processing PropertiesOriginal ValueComments
Processing Temperature 240 °C
Drying Temperature 100 - 110 °C
Dry Time 1.00 - 2.00 hour
Shelf Life 6.00 Month
 
Descriptive Properties
Chromatic valuesa.- 2,62CIELAB (D65, 10 deg)
 b.- 26,98CIELAB (D65, 10 deg)
 L.- 35,72CIELAB (D65, 10 deg)
Color index no.RAL 9005/355/PU
Light fastness7-8(1-8) blue scale, DIN 53 389

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PDANQ049 / 294469

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.