Made by suspension polymerization.
APPLICATIONS
Extrusion :
- plasticized and semi-rigid profiles and pipes
- blowing of plasticized films
Calendering : opaque or transparent, plasticized and semi-rigid films and sheets. Information provided by SolVin. SolVin is a predecessor company to Inovyn. |