MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Borealis SH950MO Polypropylene Copolymer
Categories: Polymer; Thermoplastic; Polypropylene (PP); Polypropylene Copolymer

Material Notes: SH950MO is a random heterophasic copolymer intended for injection molding. This grade yields high transparency and deep freeze impact resistance combined with excellent flow properties. The material is nucleated with Borealis Nucleation Technology (BNT). This grade contains antistatic and demolding additives which, together with enhanced nucleation, create a high potential for cycle time reduction. Products molded from this grade have an excellent balance of see-through transparency and deep freeze impact resistance. In addition, components have good gloss, very low stress whitening and excellent taste and odor properties. BNT in combination with excellent stiffness and good flow properties creates a high potential for wall-thickness reduction. CAS-No. 9010-79-1; 9002-88-4

Special Features:

  • Good flow
  • Good impact strength
  • Improved gloss and excellent transparency
  • Very low influence on taste & odor
Applications:
  • Ice cream containers
  • Crates
  • Deep freeze boxes for food storage
  • Bread boxes, crates
  • Flip top caps, high gloss closures

Information provided by Borealis AG

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.905 g/ccISO 1183
Melt Flow 40.0 g/10 min
@Load 2.16 kg,
Temperature 230 °C
ISO 1133
Storage Temperature <= 50.0 °C
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength, Yield 20.0 MPa50 mm/min; ISO 527-2
Elongation at Yield 10.0 %50 mm/min; ISO 527-2
Tensile Modulus 1050 MPa1 mm/min; ISO 527-2
Flexural Modulus 950 MPaISO 178
Charpy Impact, Notched 3.00 kJ/m²
@Temperature -20.0 °C
ISO 179/1eA
 8.00 kJ/m²
@Temperature 23.0 °C
ISO 179/1eA
 
Thermal PropertiesOriginal ValueComments
Deflection Temperature at 0.46 MPa (66 psi) 75.0 °CISO 75-2
Shrinkage 1.00 - 2.00 %
 
Processing PropertiesOriginal ValueComments
Melt Temperature 200 - 250 °C
Mold Temperature 15.0 - 40.0 °C
Hold Pressure 20.0 - 50.0 MPa

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PBORE9913 / 323270

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.