MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

(Viewing data as-entered. Click here to return)
Henkel Loctite® ECCOBOND FP4450HF Epoxy
Categories: Polymer; Thermoset; Epoxy

Material Notes: Appearance: Black

Cure: Heat Cure

Product Benefits:

  • High purity
  • Low stress
  • Good moisture resistance
  • Exhibits relatively high flow
  • High temperature performance
  • Excellent chemical resistance
Application: Encapsulant

Typical Package Application:

  • Automotive applications
  • BGA
  • IC memory cards
  • Chip carriers
  • Hybrid circuits
  • Chip-on-board
  • Multi-chip modules
  • Pin grid arrays
LOCTITE ECCOBOND FP4450 encapsulant is designed for protection of bare semiconductor devices. It offers pressure pot performance on live devices up to 500 hours with no failures, depending upon the device and package type. A cavity or potting dam is required for flow control.

Information provided by Loctite®

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.79 g/cc
Filler Content 73 %
Particle Size <= 25 µm
Brookfield Viscosity 32000 cPSpindle 6, speed 20 rpm
 
Thermal PropertiesOriginal ValueComments
CTE, linear 21.0 µm/m-°C
@Temperature 40.0 - 120 °C
Cured, Below Tg
 72.0 µm/m-°C
@Temperature 190 - 220 °C
Cured, Above Tg
Thermal Conductivity 0.620 W/m-K
@Temperature 100 °C
Cured
Maximum Service Temperature, Air 150 °C
Minimum Service Temperature, Air -65.0 °C
Glass Transition Temp, Tg 164 °CCured, by TMA
 
Processing PropertiesOriginal ValueComments
Cure Time 1.00 hour
@Temperature 110 °C
plus 3 hours @ 165°C, Alternative Cure Schedule
 30.0 min
@Temperature 125 °C
 90.0 min
@Temperature 165 °C
Gel Time 12.0 min
@Temperature 121 °C
Shelf Life 9.00 Month
@Temperature -40.0 °C
from date of manufacture
 
Descriptive Properties
Extractable Ionic Content (ppm)1Cured, Sodium (Na+)
 1Cured, Potassium (K+)
 2Cured, Chloride (Cl-)
Pot Life4 daystime to double viscosity

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PLOCT5078 / 255289

Ensinger PEI

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.